New Products /back


EN 10025-2 S355J0 high strength structural steel plate

2013年8月28日 by admin

 

Steel Grade: S355J0 ( 1.0553)

 

 

Related grades: S235JRS235J0S235J2S275JR, S275J0, S275J2S355JRS355J0S355J2, S355K2S450J0S355J0G3

 

 

S355J0 Steel Plates

S355 – a structural grade steel with a minimum yield strength of 355 N/mm² which widely used in the engineering and construction industries.

 

S355 offers high yield and tensile strength and is supplied with a variety of treatments and test options to ensure it is a highly usable steel in your various projects.

 

 

EN 10025-2 S355J0 High Yield Strength Structural Steel Plate

S symbol for Structural Steel

JR symbol 20 temperature impact test

J0 syambol 0 temperature impact test

J2 symbol -20 temperature impact test

 

 

S355J0 Characteristic

S355J0 is a low carbon, high tensile strength structural steel which can be readily welded to other weldable steel. 

With its low carbon equivalent, it possesses good cold-forming properties. The plate is produced by fully killed steel process and supplied in normalized or controlled rolling condition.

 

 

S355J0 Application 

Structural application in freight cars, transmission towers, dump trucks, cranes, trailers, bull dozers, excavators, forestry machines, railway wagons, dolphins, penstocks, pipes, highway bridges, building structures, oil and gas platforms, offshore structures, shipbuilding, power plant, palm oil equipments and machineries, fans, pumps, lifting equipments and port equipments.

 

 

Dimension we could supply: 

Thickness 8mm-300mm, Width: 1500-4020mm, Length: 3000-27000mm

 

 

S355J0 Delivery Condition: Hot rolled, CR, Normalized, Quenched, Tempering, Q+T, N+T, TMCP, Z15, Z25, Z35

 

 

S355J0 Chemical Composition(max %): 

EN

Chemical Composition

C

Si

Mn

Cr

Mo

Ni

V

N

S

P

CU

S355J0

0.24

0.60

 1.70

-

-

-

-

0.014

 0.040

0.040

0.60

 

S355J0 Mechanical Properties:

Thickness (mm)

Yield Strength Reh

min (N / mm²)

Tensile Strength Rm

min (N / mm²)

Elongation A5 min

(%)

Impact Values Charpy-V-Notch Longitudinal

Average from 3 Speimens Thk.

>10<150mm.

3<thk<100

315-335

490-630

max 22

27 Joules at 0 C

 

 

Henan Gang Iron and Steel Co. Ltd( Gangsteel) is specialized in low alloy high strength structural steel, mainly dealing with specification standard plates in EN 10025-2, EN 10025-3, EN 10025-4, EN 10025-6, ASTM A633, ASTM A573, ASTM A572, DIN 17100, JIS G3106, ASTM A709, ASTM A283, ASTM A529, ASTM A656, EN 10225, ISO 630, NFA 35-501, and so on, the thickness up to 300mm.

 

 

To find out more about S355J0 or other low alloy high strength steel, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.

Tags: EN 10025-2 S355J0  s355j0  S355J0 steel plate  s355j0 steel  EN 10025-2 S355J0  