EN 10025-2 S355K2 high strength structural steel plate

2013年8月28日 by admin

 

Steel Grade: S355K2 (1.0596)

 

 

Related grades: 

S235JRS235J0S235J2S275JR, S275J0, S275J2S355JRS355J0S355J2, S355K2S450J0S355J2G3

 

 

S355K2 Steel Plates

S355 – a structural grade steel with a minimum yield strength of 355 N/mm² which widely used in the engineering and construction industries, S355 offers high yield and tensile strength and is supplied with a variety of treatments and test options to ensure it is a highly usable steel in your various projects.

 

 

EN 10025-2 S355K2 High Yield Strength Structural Steel Plate

S355K2+N and S355K2G3 are the same steel grades as both grades delivery condition are normalized.

 

S symbol for Structural Steel

JR symbol 20 temperature impact test

J0 syambol 0 temperature impact test

J2 symbol -20 temperature impact test

K2 symbol Charpy V-Notch Impact Tested Longitudinal 40 Joules at -20 ˚C max 100mm thickness.

 

 

S355K2 Characteristic

S355K2 is a low carbon, high tensile strength structural steel which can be readily welded to other weldable steel. 

With its low carbon equivalent, it possesses good cold-forming properties. The plate is produced by fully killed steel process and supplied in normalized or controlled rolling condition.

 

 

S355K2 Application 

Structural application in freight cars, transmission towers, dump trucks, cranes, trailers, bull dozers, excavators, forestry machines, railway wagons, dolphins, penstocks, pipes, highway bridges, building structures, oil and gas platforms, offshore structures, shipbuilding, power plant, palm oil equipments and machineries, fans, pumps, lifting equipments and port equipments.

 

 

Dimension we could supply: 

Thickness 8mm-300mm, Width: 1500-4020mm, Length: 3000-27000mm

 

 

S355K2+N Delivery Condition: Hot rolled, CR, Normalized, Quenched, Tempering, Q+T, N+T, TMCP, Z15, Z25, Z35

 

 

S355K2+N Chemical Composition(max %): 

 

C

Si

Mn

Ni

P

S

Cu

max 0.24

    0.60

1.70

 

Max 0.035

Max 0.035

 0.6

 

 

S355K2+N Mechanical Properties:

Grade

Thickness (mm)

Min Yield (Mpa)

Tensile (Mpa)

Elongation (%)

Min Impact Energy

S355K2+N

8mm - 100mm

315-355 Mpa

450-630 Mpa

18-20%

-20

40J

101mm - 200mm

285-295 Mpa

450-600 Mpa

18%

-20

33J

201mm - 400mm

275 Mpa

450-600 Mpa

17%

-20

33J

The min impact energy is longitudinal energy


Henan Gang Iron and Steel Co. Ltd( Gangsteel) is specialized in low alloy high strength structural steel, mainly dealing with specification standard plates in EN 10025-2, EN 10025-3, EN 10025-4, EN 10025-6, ASTM A633, ASTM A573, ASTM A572, DIN 17100, JIS G3106, ASTM A709, ASTM A283, ASTM A529, ASTM A656, EN 10225, ISO 630, NFA 35-501, and so on, the thickness up to 300mm.

 

 

To find out more about S355K2 or other low alloy high strength steel, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.

Tags: EN 10025-2 S355K2  s355k2  EN 10025-2 S355K2  S355K2 steel  S355K2 steel plate  

0 Comments, 0 Trackbacks