New Products /back


EN 10025-2 S450J0 high strength structural steel plate

2013年8月28日 by admin

 

Steel Grade: S450J0 (1.0590)

 

 

Related grades: 

S235JRS235J0S235J2S275JR, S275J0, S275J2S355JRS355J0S355J2, S355K2S450J0S355J2G3

 

 

S450J0 Steel Plates

S450 –a structural grade steel with a minimum yield strength of 450 N/mm² which widely used in the engineering and construction industries, S450 offers high yield and tensile strength and is supplied with a variety of treatments and test options to ensure it is a highly usable steel in your various projects.

 

 

EN 10025-2 S450J0 High Yield Strength Structural Steel Plate

 

S symbol for Structural Steel

JR symbol 20 temperature impact test

J0 syambol 0 temperature impact test

J2 symbol -20 temperature impact test

 

 

S450J0 Characteristic

S450J0 is a low carbon, high tensile strength structural steel which can be readily welded to other weldable steel. 

With its low carbon equivalent, it possesses good cold-forming properties. The plate is produced by fully killed steel process and supplied in normalized or controlled rolling condition.

 

 

S450J0 Application 

Structural application in freight cars, transmission towers, dump trucks, cranes, trailers, bull dozers, excavators, forestry machines, railway wagons, dolphins, penstocks, pipes, highway bridges, building structures, oil and gas platforms, offshore structures, shipbuilding, power plant, palm oil equipments and machineries, fans, pumps, lifting equipments and port equipments.

 

 

Dimension we could supply: 

Thickness 8mm-300mm, Width: 1500-4020mm, Length: 3000-27000mm

 

 

S450JO Chemical Composition(max %):

Steel grade

C
max.
%

Mn
max.
%

 

Si 
max. 
%

 

P
max.
%

S
max.
%

N
max.
%

 

Cu
max.
%

Other
max.
%

CEV
max.
%

 

≤16

>16
≤40

>40

 

 

 

 

 

 

 

≤30

>30
≤40

>40
≤125

S450J0

0,20

0,20

0,22

1,70

0,55

0,035

0,035

0,025

0,55

-

0,47

0,49

0,49

 

S450JO Mechanical Properties:


Minimum yield strength Reh 
MPa

Tensile strength Rm 
MPa

Minimum elongation - A 
Lo = 5,65 * √So (%)

Notch impact test

Steel grade

Nominal thickness
mm

Nominal thickness
mm

Nominal thickness 
mm

Temperature

Min. absorbed energy

 

≤16

>16 
≤40

>40 
≤63

>63 
≤80

>80 
≤100

>100 
≤125

>3
≤100

>100
≤125

>3
≤40

>40
≤63

>63
≤100

>100
≤125

°C

J

S450J0

450

430

410

390

380

380

550-720

530-700

17

0

27

 

 

Henan Gang Iron and Steel Co. Ltd( Gangsteel) is specialized in low alloy high strength structural steel, mainly dealing with specification standard plates in EN 10025-2, EN 10025-3, EN 10025-4, EN 10025-6, ASTM A633, ASTM A573, ASTM A572, DIN 17100, JIS G3106, ASTM A709, ASTM A283, ASTM A529, ASTM A656, EN 10225, ISO 630, NFA 35-501, and so on, the thickness up to 300mm.

 

 

To find out more about S450J0 or other low alloy high strength steel, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.