Adopt standard:  EN10025-2

Sell steel grade: S235JR, S235J0, S235J2, S275JR, S275J0, S275J2, S355JR, S355J0, S355J2, S355K2, S450J0

 

S235J0 steel plate

 

S235JR, S235J0 and S235j2 steel is a structural steel grade which be used in riveted, bolted, or welded construction of bridges and buildings.

 

S symbol for structural steel
235 indication of the min specified yield strength for thickness of under 16mm.
JR symbol 20 temperature impact test.
J0 symbol 0 temperature impact test

J2 symbol -20 temperature impact test

 

This is common carbon steel plate in S235JR, S235J0 and S235J2 steel grade.

Gangsteel had many stock size in carbon steel plate, in ASTM A36, S235JR, S235J0, S235J2, SS400, ST37-2 and so on.

 

For more information of S235J0, please refer them in following.

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

Cu %

S235j0

0.190

-

1.500

0.040

0.040

0.014

0.060

 

 

The mechanical properties steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S235j0

8mm-100mm

215Map-235Mpa

360-510Mpa

21-26%

0

27J

101mm-200mm

195Mpa

340-500Mpa

22%

0

27J

201mm-400mm

175Mpa

21%

0

27J

The min impact energy is longitudinal energy

 

Gangsteel had many stock size in carbon steel plate, S355JR, ST52-3, A572 Gr50, S355J0 S355J2, S355J2W and so on.

If you need them more in S355JR, S235JR, S235J0, S235J2, S275JR, S275J0, S275J2, S355JR, S355J0, S355J2, S355K2, S450J0 steel grade, please contact us to get a competitive price soon.

S235j0,s235j0 steel,s235j0 grade,s235j0 material,s235j0 steel plate, s235j0 steel grade, en10025-2

 

 

Tags: s235j0  s235j0 grade  s235j0 steel  

None Comments, None Trackbacks