Sell steel grade: S275JR, S275J0, S275J2, S235JR, S235J0, S235J2, S355JR, S355J0, S355J2, S355K2, S450J0 steel grade

 

S275JR steel plate

 

 

This is common carbon steel plate in S235JR, S235J0 and S235J2 steel grade. Heat analysis shall be used to determine the required chemical composition for carbon. Manganese, phosphorus, sulfur, silicon, and copper. Tensile strength, yield strength, and elongation shall be evaluated using tension test.

 

S symbol for structural steel
275 indication of the min specified yield strength for thickness of under 16mm.
JR symbol 20 temperature impact test.
J0 symbol 0 temperature impact test

J2 symbol -20 temperature impact test

 

 

S275JR, S275J0 and S275j2 steel is a structural steel grade which be used in riveted, bolted, or welded construction of bridges and buildings.

 

For more information of S275jr steel, please refer them in following.

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

Cu %

S275JR

0.240

-

1.600

0.045

0.045

0.014

0.060

 

 

The mechanical properties steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S275JR

8mm-100mm

275Mpa

430-560Mpa

21-23%

20

27J

101mm-200mm

225-235Mpa

400-540Mpa

19%

20

27J

201mm-400mm

215Mpa

380-540Mpa

18%

20

27J

The min impact energy is longitudinal energy

 

If you need them more, you could check them in our website of stock warehouse or contract us by email.

Our mill sells S275JR, S275J0, S275J2, S235JR, S235J0, S235J2, S355JR, S355J0, S355J2, S355K2, S450J0, S275JR, S275J0 and S275J2 in EN10025-2 standard.


If you have any order in this steel grade from gangsteel, please inquiry us soon.

 

S275jr,s275jr steel,s275jr steel plate,s275jr grade,s275jr steel grade,en10025-2

 

 

 

 

Tags: S275JR  S275jr steel  s275jr material  

0 Comments, 0 Trackbacks