New Products /back


s355jr en10025-2 s355jr steel plate s355jr material

2011年4月5日 by admin

S355jr,s355jr steel,s355jr grade,s355jr steel plate,s355jr steel grade,en10025-2

 

Adopt standard:  EN10025-2

Sell steel grade: S355JR, S235JR, S235J0, S235J2, S275JR, S275J0, S275J2, S355J0, S355J2, S355K2, S450J0 steel grade,s355j2g3,s355j2n,s355j2+n steel

 

S355JR steel plate

 

 

S355JR steel is a more yield and tensile strength steel grade than S235JR and S275JR. it is used to be in in riveted, bolted, or welded construction of bridges and buildings.

 

S355JR mean that the delivery station is hot rolled or control rolled. If super thick steel plate, gangsteel also could do in normalized by using ingot to satisfy requirement from customers

 

Gangsteel is specialized in supply S355JR steel grade. If you need more low temperature impact test, you could choose S355J0 or S       355J2 Which has a 0 or -20 degree impact test.

 

For more information of S355JR, please refer them in following.

 

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

Cu %

S355JR

0.270

0.600

1.700

0.045

0.045

0.014

0.060

 

 

 

 

The mechanical properties steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S355JR

8mm-100mm

315Map-355Mpa

450-630Mpa

18-20%

20

27J

101mm-200mm

285Mpa-295Mpa

450-600Mpa

18%

20

27J

201mm-400mm

275Mpa

17%

20

27J

The min impact energy is longitudinal energy

 

Gangsteel had many stock size in carbon steel plate, S355JR, ST52-3, A572 Gr50, S355J0 S355J2, S355J2W and so on. Please check some parts of stock size in following.

 

If you need them more in S355JR, or S355JR, S235JR, S235J0, S235J2, S275JR, S275J0, S275J2, S355J0, S355J2, S355K2, S450J0 steel grade,s355j2g3,s355j2n,s355j2+n steel please contact us soon.

 

S355jr,s355jr steel,s355jr grade,s355jr steel plate,s355jr steel grade,en10025-2

 

Tags: s355jr  en10025  s355j0  s355jr steel  

0 Comments, 0 Trackbacks