S355K2G3 EN10025-2 S355K2G3 steel plate

2011年4月5日 by admin

S355k2g3, s355k2g3 steel, s355k2g3 grade, s355k2g3 steel grade, s355k2g3 steel plate, en10025-2, s355k2g3

 

Adopt standard:  EN10025-2

Sell steel grade: S355K2, S235JR, S235J0, S235J2, S275JR, S275J0, S275J2, S355JR, S355J0, S355J2, S450J0 steel

 

S355K2G3 steel plate

 

 

S355K2G3 steel plate has a -20 degree temperature steel. Compare with S355J2 , S355K2 steel plate impact energy is 40J, S355J2 is 27J under 150mm thickness.
So S355K2 steel plate is better for choice in low temperature high impact energy projects.

 

Gangsteel is specialized in supplying S355K2G3 steel grade in super thick steel plate. We exported our goods to Vietnam, Korea and Singapore in this grade in many years. Gangsteel promised that we used our best service to enlarge steel market of oversea.

 

If you need more yield and tensile strength, you could choose S450J0 steel grade Which has min 450Mpa yield strength.

 

For more information S355K2G3, please refer them in following.

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

Cu %

S355K2G3

0.23-0.24

0.600

1.700

0.035

0.035

0.060

 

 

The mechanical properties steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S355K2G3

8mm-100mm

315Map-355Mpa

450-630Mpa

18-20%

-20

40J

101mm-200mm

285Mpa-295Mpa

450-600Mpa

18%

-20

33J

201mm-400mm

275Mpa

450-600Mpa

17%

-20

33J

The min impact energy is longitudinal energy

 

Gangsteel had many stocks in carbon steel plate, for S355K2G3 and S450J0, we suggest you to order new goods because this grade is hard to find stock in steel market of China

 

If you have any inquiry in S355K2G3 steel plate, or S355K2, S235JR, S235J0, S235J2, S275JR, S275J0, S275J2, S355JR, S355J0, S355J2, S450J0 steel, please feel free to contact us by email or calling.

 

S355k2g3, s355k2g3 steel, s355k2g3 grade, s355k2g3 steel grade, s355k2g3 steel plate, en10025-2, s355k2g3

 

 

Tags: s355k2g3  en10025  s355k2g3 steel  

0 Comments, 0 Trackbacks