New Products /back


EN 10025-3 S355NL,S355NL steel,S355NL steel plate,S355nl supplier

2013年8月26日 by admin

Adopt standard: EN10025-3 S355NL

 S355N steel is a structural steel grade. S means structural steel, 355 means min yield strength for thickness less 16mm expressed in Mpa, NL mean the delivery condition.
 
Compare the S275N/s275NL, S355NL steel has a more yield and tensile strength. The equal grade of S355NL is S355ML.
 
Gangsteel could provide max thickness to 350mm by using ingot. Max width 3800mm, we also could do the UT test, impact test, Chemical analysis, mechanical test, and Simulated may treatment according to our customer requirement.
 
 
About S355NL steel detail information, please refer to technical date in following.
 
The Chemical is max composition of product analysis:
 

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
0.180
0.500
0.9-1.65
0.025
0.020
0.120
0.020
0.300
Cu %
Mo %
Nb %
Ni %
Ti %
N %
 
 
0.550
0.100
0.050
0.300
0.050
0.015
 
 

 
 
The mechanical properties steel plate
 
 

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
S355NL
8mm-100mm
235Map-275Mpa
470-630Mpa
22%
-50
27J
101mm-200mm
285Mpa-315Mpa
450-600Mpa
21%
-50
27J
201mm-250mm
275Mpa-285Mpa
450-600Mpa
21%
-50
27J
The min impact energy is longitudinal energy

 
 
 
For more information in quality certificate or inquiry in competitive official quotation, please contact us by email.
 

Tags: EN 10025-3 S355NL  s355nl  s355nl steel  S355nl steel plate  S355nl supplier  

0 Comments, 0 Trackbacks