S355N Steel Plate

Adopt standard: EN10025-3

 

Sell steel grade: S275N steel,S355N steel,S420N steel,S460N steel,S275NL steel,S355NL steel,S420NL steel,S460NL steel

 

S355N Steel Grade

 

S355N steel is a structural steel grade. S means structural steel, 355 means min yield strength for thickness less 16mm expressed in Mpa, N mean the delivery condition.

Compare the S275N/s275NL, S355N steel has a more yield and tensile strength. The equal grade of S355N is S355M.

 

Gangsteel could provide max thickness to 350mm by using ingot. Max width 3800mm, we also could do the UT test, impact test, Chemical analysis, mechanical test, and Simulated may treatment according to our customer requirement.

 

 

About S355N steel detail informationplease refer to technical date in following.

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

V %

AL %

Cr %

S355N

0.200

0.500

0.9-1.65

0.030

0.025

0.120

0.020

0.300

Cu %

Mo %

Nb %

Ni %

Ti %

N %

 

 

0.550

0.100

0.050

0.300

0.050

0.015

 

 

 

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

 

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S355N

8mm-100mm

235Map-275Mpa

470-630Mpa

22%

-20

40J

101mm-200mm

285Mpa-315Mpa

450-600Mpa

21%

-20

40J

201mm-250mm

275Mpa-285Mpa

450-600Mpa

21%

-20

40J

The min impact energy is longitudinal energy

 

 

 