Sell steel grade: S275N, S355N, S420N, S460N, S275NL, S355NL, S420NL,S460NL steel plate

 

S420NL Steel plate

 

S420NL steel is a good weldability structural steel grade. General requirements for arc welding of the steels specified shall be as given in EN 1011-2.

 

Compare the S355N, S420NL steel grade has more yield and tensile strength. The equal grade of S420NL is S420ML.

 

Gangsteel has much experience in manufacture S420NL. we cooperated with wuyang mill of HBIS to produce the max thickness 300mm in electroslag remelting technical. Our advantage is that we could supply goods in the fastest delivery time, even in one plate in usual specification.

 

 

About S420NL steel detail informationplease refer to technical date in following.

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

V %

AL %

Cr %

S420NL

0.200

0.600

1.0-1.7

0.025

0.030

0.020

0.020

0.300

Cu %

Mo %

Nb %

Ni %

Ti %

N %

 

 

0.550

0.100

0.050

0.800

0.050

0.025

 

 

 

 

 

The mechanical properties:

 

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S420NL

8mm-100mm

360Map-420Mpa

520-680Mpa

19%

-50

27J

101mm-200mm

330Mpa-360Mpa

500-650Mpa

18%

-50

27J

201mm-250mm

320Mpa-330Mpa

500-650Mpa

18%

-50

27J

The min impact energy is longitudinal energy

 

 

 

For more information in S420NL quality certificate or inquiry in competitive official quotation, please contact us by email.

 

 

Tags: S420nl material  s420nl  s420nl steel  

0 Comments, 0 Trackbacks