S275M EN10025-4 S275M steel plate
2011年4月5日 by admin
EN10025-4,S275M,S275M steel,S275M steel grade,S275M steel plate.
Adopt Standard EN10025-4
Gang steel Grade:
EN10025-4 | S275M | S275ML | S355M | S355ML |
Grade | S420M | S420ML | S460M | S460ML |
S275M steel plate
S275M Grade is a technical delivery conditions for thermo mechanical rolled weldable fine grain structural steels.
S means the structural steel, M means the delivery condition.
Capital letter L for the quality with specified minimum values of values of impact energy at temperature not lower than -50 degree.
Gangsteel is a large agent of HBIS wuyang mill in
S275M Chemical composition of the product analysis for thermo mechanical rolled steel
Element | S275M Max % | Element | S275M max % |
C | 0.15 | | 0.015 min |
Si | 0.55 | TI | 0.06 |
Mn | 1.60 | CR | 0.35 |
P | 0.035 | NI | 0.35 |
S | 0.030 | Mo | 0.13 |
Nb | 0.06 | Cu | 0.60 |
V | 0.10 | N | 0.017 |
S275M Mechanical properties at ambient temperature for thermo mechanical rolled steel
Grade | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | -20 degree | |
S275M | ≤ 16 | 275 | 370-530 | 24 | 40 |
16> to ≤40 | 265 | 370-530 | 24 | 40 | |
40> to ≤63 | 255 | 350-510 | 24 | 40 | |
63> to ≤80 | 245 | 350-510 | 24 | 40 | |
80> to ≤100 | 245 | 350-510 | 24 | 40 | |
100> to ≤120 | 240 | 350-510 | 24 | 40 |
If you want to find our stock in S275M, or inquiry S275M from our Gangsteel, please feel free to contact us by email or calling.