S420ML Grade is a technical delivery conditions for thermo mechanical rolled weldable fine grain structural steels.
S means the structural steel, M means the delivery condition.
Capital letter L for the quality with specified minimum values of values of impact energy at temperature not lower than -50 degree.

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick S420ML steel plate. We could supply the min order is a piece and promise the competitive price in order to enlarge our oversea market.

S420ML Chemical composition of the product analysis for thermo mechanical rolled steel

Element

S420ML  Max %

Element

S420ML max %

C

0.18

AL

    0.015 min

Si

0.55

TI

0.06

Mn

1.80

CR

0.35

P

0.030

NI

0.85

S

0.025

Mo

0.23

Nb

0.06

Cu

0.60

V

0.14

N

0.027

 

S420ML Mechanical properties at ambient temperature for thermo mechanical rolled steel

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-50 degree

S420ML

≤ 16

 420

520-680

19

27

16> to ≤40

    400

520-680

19

27

40> to ≤63

 390

500-660

19

27

63> to ≤80

 380

480-640

19

27

80> to ≤100

 370

470-630

19

27

100> to ≤120

 365

460-620

19

27

 

If you want to find our stock in S420ML, or inquiry S420ML from our Gangsteel, please feel free to contact us by email or calling.

EN10025-4,S420ML,S420ML steel,S420ML steel grade,S420ML steel plate.

 

 

Tags: s420ml  en10025 s420ml  s420ml steel  

0 Comments, 0 Trackbacks