New Products /back


S235J0W,S235J0W steel,S235J0W steel plate

2011年4月14日 by admin

S235J0W,S235J0W steel,S235J0W grade,S235J0W steel grade,S235J0W steel plate,S235J0W

 

Adopt Standard: BS EN10025-5
Gangsteel steel grade: S235J0W,S235J2W, S355J0WP,S355J2WP,S355J0W,S355J2W,S355K2W

 

S235J0W steel plate

 

 

 

S235J0W steel grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.

 

S mean S235J0W grade could be used in structural steel projects, 235 is the min yield strength.

J0 ,J2 and K2 standard for the impact degree and energy in 0 temperature.

W means that the mainly different in their carbon and phosphorus contents and availability.

 

For the steel grade in S235 a maximum carbon equivalent value of 0.44% and for grade s355 a maximum carbon equivalent value of 0.52% based on the ladle analysis shall for all thickness.

 

Gangsteel is specialized in improved atmospheric corrosion resistance steel grade. We exported the grade Corten A and Corten B, 09CuPCrNi-A,09CuPCrNi-B grade, 05CuPCrNi-A steel, and A588 Grade K, A588 Grade A steel.

 

S235J0W steel Chemical composition in Product analysis

 

Carbon, %

 

Manganese, %

Cr %

Silicon %

N % max

Sulfur %

Max  0.16

 

0.15-0.70

0.35-0.85

Max 0.45

0.010

0.040-0.035

Cu  %

 

Phosphorus %

 

 

 

 

0.20-0.60

 

Max 0.040

 

 

 

 

 

S235J0W steel Mechanical Properties

Grade

Min. Yield Strength Mpa

Tensile Strength MPa

Impact

S235J0W

Nominal Thickness (mm)

Nominal Thickness (mm)

degree

J

Thick mm

≤16

>16

≤40

>40

≤63

>63

≤80

>80

≤100

>100

≤150

≤3

>3 ≤100

>100 ≤150

 

 

0

 

 

27

S235J0W

235

225

215

215

215

195

360-510

360-510

350-500

 

 

 

Any need in S235J0W steel grade, please feel free to contact us by email or calling to us, we will reply our competitive price to you soon.

S235J0W,S235J0W steel,S235J0W grade,S235J0W steel grade,S235J0W steel plate,S235J0W

 

 

Tags: S235J0W  S235J0W steel  S235J0W grade  S235J0W steel grade  S235J0W steel plate  S235J0W  

0 Comments, 0 Trackbacks