New Products /back


S355J0W,S355J0W steel,S355J0W grade,en10025-5

2011年4月14日 by admin

S355J0W,S355J0W steel,S355J0W grade,S355J0W steel grade,S355J0W steel plate,S355J0W

 

Adopt Standard: BS EN10025-5
Gangsteel steel grade: S235J2W,S235J0W, S355J0WP,S355J2WP,S355J0W,S355J2W,S355K2W

 

S355J0W steel plate

 

 

 

S355J0W steel grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.

 

S mean S355J0W grade could be used in structural steel projects, 235 is the min yield strength.

J0 ,J2 and K2 standard for the impact degree and energy in 0 temperature.

W means that the mainly different in their carbon and phosphorus contents and availability.

 

For the steel grade in S235 a maximum carbon equivalent value of 0.44% and for grade s355 a maximum carbon equivalent value of 0.52% based on the ladle analysis shall for all thickness.

 

Gangsteel is specialized in improved atmospheric corrosion resistance steel grade. We exported the grade Corten A and Corten B, 09CuPCrNi-A,09CuPCrNi-B grade, 05CuPCrNi-A steel, and A588 Grade K, A588 Grade A steel.

 

S355J0W steel Chemical composition in Product analysis

 

Carbon, %

Manganese, %

Cr %

Silicon %

N % max

Sulfur %

Max  0.19

0.45-1.60

0.35-0.85

Max 0.55

0.010

Max 0.040

Cu  %

Phosphorus %

N %

 

 

 

0.20-0.60

Max 0.040

0.010

 

 

 

 

S355J0W steel Mechanical Properties

Grade

Min. Yield Strength Mpa

Tensile Strength MPa

Impact

S355J0W

Nominal Thickness (mm)

Nominal Thickness (mm)

degree

J

Thick mm

≤16

>16

≤40

>40

≤63

>63

≤80

>80

≤100

>100

≤150

≤3

>3 ≤100

>100 ≤150

 

 

0

 

 

27

S355J0W

355

345

335

325

315

295

510-680

470-630

450-600

 

 

Any need in S355J0W steel grade, please feel free to contact us by email or calling to us, we will reply our competitive price to you soon.