New Products /back


S355J0WP,S355J0WP steel,S355J0WP steel plate,en10025-5

2011年4月14日 by admin

S355J0WP,S355J0WP steel,S355J0WP grade,S355J0WP steel grade,S355J0WP steel plate,S355J0WP

 

Adopt Standard: BS EN10025-5
Gangsteel steel grade: S235J2W,S235J0W, S355J0WP,S355J2WP,S355J0W,S355J2W,S355K2W

 

S355J0WP steel plate

 

 

 

S355J0WP steel grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.

 

S mean S355J0WP grade could be used in structural steel projects, 235 is the min yield strength.

J0 ,J2 and K2 standard for the impact degree and energy in 0 temperature.

W means that the mainly different in their carbon and phosphorus contents and availability.

 

For the steel grade in S235 a maximum carbon equivalent value of 0.44% and for grade s355 a maximum carbon equivalent value of 0.52% based on the ladle analysis shall for all thickness.

 

Gangsteel is specialized in improved atmospheric corrosion resistance steel grade. We exported the grade Corten A and Corten B, 09CuPCrNi-A,09CuPCrNi-B grade, 05CuPCrNi-A steel, and A588 Grade K, A588 Grade A steel.

 

S355J0WP steel Chemical composition in Product analysis

 

Carbon, %

 

Manganese, %

Cr %

Silicon %

N % max

Sulfur %

Max  0.15

 

Max 1.1

0.25-1.35

Max 0.8

0.010

0.040-0.035

Cu  %

 

Phosphorus %

N %

 

 

 

0.20-0.60

 

0.05-0.16

0.010

 

 

 

 

S355J0WP steel Mechanical Properties

Grade

Min. Yield Strength Mpa

Tensile Strength MPa

Impact

S355J0WP

Nominal Thickness (mm)

Nominal Thickness (mm)

degree

J

Thick mm

≤16

>16

≤40

>40

≤63

>63

≤80

>80

≤100

>100

≤150

≤3

>3 ≤100

>100 ≤150

 

 

0

 

 

27

S355J0WP

355

345

….

….

….

….

510-680

470-630

….

 

 

Any need in S355J0WP steel grade, please feel free to contact us by email or calling to us, we will reply our competitive price to you soon.

S355J0WP, S355J0WP steel,S355J0WP grade,S355J0WP steel grade,S355J0WP steel plate,S355J0WP

 

 

Tags: S355J0WP  S355J0WP steel  S355J0WP grade  S355J0WP steel grade  S355J0WP steel plate  S355J0WP  