S355J2W,S355J2W steel,S355J2W steel plate,En10025-5
2011年4月14日 by admin
S355J2W,S355J2W steel,S355J2W grade,S355J2W steel grade,S355J2W steel plate,S355J2W
Adopt Standard: BS EN10025-5
Gangsteel steel grade: S235J2W,S235J0W, S355J2WP,S355J2WP,S355J0W,S355J2W,S355K2W
S355J2W steel plate
S355J2W steel grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.
S mean S355J2W grade could be used in structural steel projects, 235 is the min yield strength.
J0 ,J2 and
W means that the mainly different in their carbon and phosphorus contents and availability.
For the steel grade in S
Gangsteel is specialized in improved atmospheric corrosion resistance steel grade. We exported the grade Corten A and Corten B, 09CuPCrNi-A,09CuPCrNi-B grade, 05CuPCrNi-A steel, and A588 Grade K, A588 Grade A steel.
S355J2W steel Chemical composition in Product analysis
Carbon, % | | Manganese, % | Cr % | Silicon % | N % max | Sulfur % |
Max 0.19 | | 0.45-1.60 | 0.35-0.85 | Max 0.55 | …. | Max 0.035 |
Cu % | | Phosphorus % | N % | | | |
0.20-0.60 | | Max 0.035 | 0.010 | | | |
S355J2W steel Mechanical Properties
Grade | Min. Yield Strength Mpa | Tensile Strength MPa | Impact | ||||||||
S355J2W | Nominal Thickness (mm) | Nominal Thickness (mm) | degree | J | |||||||
Thick mm | ≤16 | >16 ≤40 | >40 ≤63 | >63 ≤80 | >80 ≤100 | >100 ≤150 | ≤3 | >3 ≤100 | >100 ≤150 | -20 | 27 |
S355J2W | 355 | 345 | 335 | 325 | 315 | 295 | 510-680 | 470-630 | 450-600 |
Any need in S355J2W steel grade, please feel free to contact us by email or calling to us, we will reply our competitive price to you soon.
S355J2W, S355J2W steel,S355J2W grade,S355J2WP steel grade,S355J2W steel plate,S355J2W
Tags: S355J2W S355J2W steel S355J2W grade S355J2W steel grade S355J2W steel plate S355J2W