New Products /back


S500QL1,S500QL1 Grade,S500QL1 steel plate,EN10025-6 S500QL1

2011年3月22日 by admin

S500QL1,S500QL1 Grade,S500QL1 steel plate,EN10025-6 S500QL1

S500Q/QL/QL1 steel plate from Gangsteel

Adopt standard: S500QL1 EN 10025-6
Sell steel grade: S500Q steel plate, S500QL steel plate, S500QL1 steel plate
 
S500Q/QL/QL1 Steel Grade
 
S500Q S500QL and S500QL1 high yield strength structural steels grade in the quenched and tempered.
 
In the low-temperature impact: S500Q steel plate -20 30J, S500QL steel plate -40 30J, S500QL1 steel plate -60 30J.

 
 
Our Company can supply the S500Q, S500QL and S500QL1 steel plate directly from our mill in the competitive price for our long cooperation. We also could cut large plate to the size or shape you require.

About S500Q/QL/QL1 detail information,please consult technical date in following.
 
The Chemical is max composition of product analysis:
 

Grade
C %
Si %
Mn %
P %
S %
N %
B %
Cr %
 
S500QL
 
0.200
0.800
1.700
0.020
0.010
0.015
0.005
1.500
Cu %
Mo %
Nb %
Ni %
Ti %
V %
Zr %
 
0.500
0.700
0.060
2.000
0.050
0.120
0.150
 

 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate
 

Grade
Thickness
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
S500QL
8mm-50mm
Min 500Mpa
590-770Mpa
17%
-40
Min 30J
51mm-100mm
Min 480Mpa
590-770Mpa
17%
-40
Min 30J
101mm-150mm
Min 440Mpa
540-720Mpa
17%
-40
Min 30J

 
 
 
If you have any need in S500Q/QL/QL1 steel plates,please feel free to contact us by email or mobile.
 
 

Tags: S500QL1  S500QL1 Grade  S500QL1 steel plate  EN10025-6 S500QL1  