S460Q/QL/QL1 steel plate

2011年3月30日 by admin

 

S460Q/QL/QL1 steel plate from Gangsteel

 

Adopt standard: S460Q EN 10025-6

Sell steel grade: S460Q steel plate, S460QL steel plate, S460QL1 steel plate

 

S460Q/QL/QL1 Steel Grade

 

S460Q S460QL and S460QL1 high yield strength structural steels grade in the quenched and tempered and

S460Q/QL/QL1 steel plate could be used in Mechanical Engineeringsuspension arm and others parts in machine.

If you need more yield strength, you could choose our others grade in S690Q, S890Q or S960Q

 

Gangsteel sell S460Q S460QL and S460QL1 EN 10025-6 steel plates directly from our mill. Gangsteel are special field of exporting steel plate on base of large relation with our mill in China.

 

.About S460Q/QL/QL1 detail information, please consult technical date in following.

 

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

B %

Cr %

 

S460Q

 

0.200

0.800

1.700

0.030

0.017

0.015

0.005

1.500

Cu %

Mo %

Nb %

Ni %

Ti %

V %

Zr %

 

0.500

0.700

0.060

2.000

0.050

0.120

0.150

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S460Q

8mm-50mm

Min 460Mpa

550-720Mpa

17%

-20

Min 30J

51mm-100mm

Min 440Mpa

550-720Mpa

17%

-20

Min 30J

101mm-150mm

Min 400Mpa

500-670Mpa

17%

-20

Min 30J

 

 