New Products /back


S500Q/QL/QL1 steel plate

2011年3月30日 by admin

S500Q/QL/QL1 steel plate from Gangsteel

 

Adopt standard: S500QL1 EN 10025-6

Sell steel grade: S500Q steel plate, S500QL steel plate, S500QL1 steel plate

 

S500Q/QL/QL1 Steel Grade

 

S500Q S500QL and S500QL1 high yield strength structural steels grade in the quenched and tempered.

 

In the low-temperature impact: S500Q steel plate -20 30J, S500QL steel plate -40 30J, S500QL1 steel plate -60 30J.

 

Our Company can supply the S500Q, S500QL and S500QL1 steel plate directly from our mill in the competitive price for our long cooperation. We also could cut large plate to the size or shape you require.


About S500Q/QL/QL1 detail information
please consult technical date in following.

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

B %

Cr %

 

S500QL

 

0.200

0.800

1.700

0.020

0.010

0.015

0.005

1.500

Cu %

Mo %

Nb %

Ni %

Ti %

V %

Zr %

 

0.500

0.700

0.060

2.000

0.050

0.120

0.150

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

 

Grade

Thickness

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S500QL

8mm-50mm

Min 500Mpa

590-770Mpa

17%

-40

Min 30J

51mm-100mm

Min 480Mpa

590-770Mpa

17%

-40

Min 30J

101mm-150mm

Min 440Mpa

540-720Mpa

17%

-40

Min 30J

 

 

 

If you have any need in S500Q/QL/QL1 steel platesplease feel free to contact us by email or mobile.

 

 

 

Tags: S500Q  S500QL  S500QL1  