S550Q/QL/QL1 steel plate

2011年3月30日 by admin

S550Q/QL/QL1 steel plate from Gangsteel

 

Adopt standard: S550Q EN 10025-6

Sell steel grade: S550Q steel plate, S550QL steel plate, S550QL1 steel plate

 

S550Q/QL/QL1 Steel Grade

 

S550Q S550QL and S550QL1 high yield strength structural steels grade in the quenched and tempered.

S550Q/QL/QL1 steel plate has better weldability. General requirements for arc welding of the steels specified shall be as given in EN 1011-2.

S550Q/QL/QL1 steel plate could be used in Mechanical Engineering, suspension arm and others parts in machine.

 

Gangsteel supply S550Q S550QL and S550QL1 EN 10025-6 steel plates directly from our mill. besides that, we also have many stock in hand in large thickness. Gangsteel sincerely hope new and old customers could inquiry our steel plates.


About S550Q/QL/QL1 detail information
please consult technical date in following.

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

B %

Cr %

 

S550Q

 

0.200

0.800

1.700

0.030

0.017

0.015

0.005

1.500

Cu %

Mo %

Nb %

Ni %

Ti %

V %

Zr %

 

0.500

0.700

0.060

2.000

0.050

0.120

0.150

 

 

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S550Q

8mm-50mm

Min 550Mpa

640-820Mpa

16%

-20

Min 30J

51mm-100mm

Min 530Mpa

640-820Mpa

16%

-20

Min 30J

101mm-150mm

Min 490Mpa

590-770Mpa

16%

-20

Min 30J

 

 

 

If you have any need in S550Q/QL/QL1 steel platesplease feel free to contact us by email or mobile.

 

 