Adopt standard:  S890QL1 steel EN 10025-6

Sell steel grade: S890Q steel plate, S890QL steel plate, S890QL1 steel plate

 

S890QL1 steel grade

 

S890QL1 is good weld-ability, -60 temperature impact test in 30J in quenched and tempered steel.

 

The symbol S for structural steel, 890 mean the minimum yield strength in thickness under 50mm.

Q mean the delivery condition in quenched and tempered.

S890QL1 steel could be through the -60 temperature impact and the energy is 30J, which could be used in lower temperature environment.

 

Gangsteel have many years experience in exporting S890QL1 steel plates. We will use our specialized knowledge, perfected service and fastest delivery to build our long cooperation in business. if you have any need in steel platesplease contact us.

 

About S890QL1 steel detail informationplease refer to our mill technical date in following:

 

 

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

B %

Cr %

S890QL1

0.200

0.800

1.700

w

0.010

0.015

0.005

1.500

Cu %

Mo %

Nb %

Ni %

Ti %

V %

Zr %

 

0.500

0.700

0.060

2.000

0.050

0.120

0.150

 

 

 

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

 

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S890QL1

8mm-50mm

Min 890Mpa

940-1100Mpa

11%

-60

Min 30J

51mm-100mm

Min 830Mpa

880-1100Mpa

11%

-60

Min 30J

101mm-150mm

Min 800Mpa

820-1000Mpa

11%

-60

Min 30J

 

 