New Products /back


S960QL steel plate

2011年3月30日 by admin

S960QL steel plate from Gangsteel

 

Adopt standard: S960Q EN 10025-6

Sell steel grade: S960Q steel plate, S960QL steel plate

 

S960L Steel Grade


S960QL steel is high yield strength structural steels in the quenched and tempered delivery state.

 

For S960QL steel plate tolerance the basic requirements shall be in according with EN 10029, including thickness tolerances to class A, unless otherwise agreed at the time of the order.


S960QL steel plate could be through the -40 temperature impact and the energy is 30J.

 

Gangsteel Company sells S960QL steel plate sickly according to EN10025-6 Standard for our customers. our mill have many years experience in S960QL steel manufacturing technique.

 

 

For S960QL steel detail informationplease refer to our mill technical date in following:

 

The Chemical of S960QL is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

B %

Cr %

S960QL

0.200

0.800

1.700

0.025

0.015

0.015

0.005

1.500

Cu %

Mo %

Nb %

Ni %

Ti %

V %

Zr %

 

0.500

0.700

0.060

2.000

0.050

0.120

0.150

 

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate s960ql

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S960QL

8mm-50mm

Min 960Mpa

980-1150Mpa

10%

-40

Min 30J

51mm-100mm

Min 910Mpa

920-1000Mpa

10%

-40

Min 30J

101mm-150mm

Min 860Mpa

870-980Mpa

10%

-40

Min 30J

 

 

 