New Products /back


S890Q steel plate

2011年3月30日 by admin

S890Q steel plate from Gangsteel

 

Adopt standard:  S890Q steel EN 10025-6

Sell steel grade: S890Q steel plate, S890QL steel plate, S890QL1 steel plate

 

S890Q steel plate

 

S890Q steel grade is a high strength, and toughness steel in min yield strength 890Mpa, -20 temperature impact energy 30J in quenched and tempered delivery station.

 

 

S890Q steel plate has better weldability. General requirements for arc welding of the steels specified shall be as given in EN 1011-2.

S890Q could be used in Mechanical Engineeringsuspension arm and others parts in machine.

 

Gangsteel supply S890Q EN 10025-6 steel plates directly from our mill in the competitive price.

 

We sincerely hope customer could come to our mill and factory to inspect our quality and ability in manufacture for our long cooperation.

About S890Q detail information, please refer to our mill technical date in following:

 

The Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

N %

B %

Cr %

S890Q

0.200

0.800

1.700

0.025

0.015

0.015

0.005

1.500

Cu %

Mo %

Nb %

Ni %

Ti %

V %

Zr %

 

0.500

0.700

0.060

2.000

0.050

0.120

0.150

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S890Q

8mm-50mm

Min 890Mpa

940-1100Mpa

11%

-20

Min 30J

51mm-100mm

Min 830Mpa

880-1100Mpa

11%

-20

Min 30J

101mm-150mm

Min 800Mpa

820-1000Mpa

11%

-20

Min 30J

 

 

Gangsteel are special field of exporting steel plate on base of large relation with our HBIS Wuyang mill in China. If you have any inquiry in steel plates, Please feel free to contact us.

 

 

 

Tags: S890Q steel plate  

0 Comments, 0 Trackbacks