EN10028-2 P265GH boiler and pressure vessel steel plate

2013年9月11日 by admin

EN10028-2 P265GH boiler and pressure vessel steel plate

 

Related Grade:P235GH,p265gh,p295gh,p355gh,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4, 20MnMoNi4-5,15NiCuMoNb5-6-4,

13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.

 

P265GH steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.

 

In accordance with en10020, P235GH,p265gh, p295gh and p355gh are non alloy quality steels.

 All of other grade are alloy special steels.

 

P265GH Grade delivery condition is normalizing or be replaced with normalizing rolling at the discretion of manufactures. 

 

Gangsteel could supply P265GH steel grade in super thick steel plate for fabricators serving the oil and gas industry, 

heat exchangers, weldable pressure vessels and boilers

 

Steel ServicesCutting, Painting, Pretreatment, Ultrasonic Test, Third Party Inspection, HIC, NACE, and so on.

 

P265GH Chemical composition cast analysis

Element

P265GH  Max %

Element

P265GH max %

C

0.20

Cr

0.30

Si

0.40

Cu

0.30

Mn

0.80-1.40

Mo

0.08

P

0.025

Nb

0.020

S

0.015

Ni

0.30

AL

0.020 min

Ti

0.30

N

0.012

V

0.02


 

P265GH Mechanical properties 

Condition

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

Normalized

≤ 16

265

410-530

22

27

16> to ≤40

   255

410-530

22

27

40> to ≤60

245

410-530

22

27

60> to ≤100

215

410-530

22

27

100> to ≤150

200

400-530

22

27

150> to ≤250

185

390-530

22

27


 