New Products /back


12CrMo9-10,EN10028-2,12CrMo9-10 steel plate

2011年4月14日 by admin

EN10028-2,12CrMo9-10,12CrMo9-10,12CrMo9-10,12CrMo9-10

 

Adopt Standard: EN10028-2

Grade:P235GH,P265GH,P295GH,P355GH,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4,20MnMoNi4-5,15NiCuMoNb5-6-4,13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.

 

12CrMo9-10 steel grade

12CrMo9-10 steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.

In accordance with en10020, 12CrMo9-10 steel grade is alloy special steels.

12CrMo9-10 Grade delivery condition is normalized and tempered or quenched and tempered.

 

Gangsteel could supply 12CrMo9-10 steel grade in super thick steel plate for fabricators serving the oil and gas industry, heat exchangers, weldable pressure vessels and boilers

For more information in 12CrMo9-10 steel grade in the following:


12CrMo9-10 Chemical composition cast analysis

Element

12CrMo9-10  Max %

Element

12CrMo9-10 max %

C

0.10-0.15

Cr

2.00-2.25

Si

0.30

Cu

0.25

Mn

0.30-0.80

Mo

0.90-1.10

P

0.015

Nb

 

S

0.010

Ni

0.30

AL

0.010-0.040

Ti

 

N

0.012

V

 

 

12CrMo9-10 Mechanical properties

Grade

Condition

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

12CrMo9-10

+NT or +QT

≤ 16

355

540-690

18

27

16> to ≤40

  355

540-690

18

27

40> to ≤60

355

540-690

18

27

60> to ≤100

355

540-690

18

27

100> to ≤150

355

540-690

18

27

150> to ≤250

355

540-690

18

27

Noted: +NT mean Normalized and tempered; +QT mean Quenched and tempered

 

If you want to find our stock in 12CrMo9-10 or inquiry from our gangsteel, please feel free to contact us by email or calling.

 

Tags: EN10028-2  12CrMo9-10  12CrMo9-10 steel  12CrMo9-10  12CrMo9-10  