Adopt Standard: EN10028-2
Grade:P235GH,P265GH,P295GH,P355GH,16Mo3,18MnMo4-5,20MnMoNi4-5,13CrMoV9-10,20MnMoNi4-5,13CrMoV9-10,13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.
13CrMoV9-10 steel grade
13CrMoV9-10 steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.
In accordance with en10020, 13CrMoV9-10 steel grade is alloy special steels.
13CrMoV9-10 Grade delivery condition is normalized and tempered or quenched and tempered.
Gangsteel could supply 13CrMoV9-10 steel grade in super thick steel plate for fabricators serving the oil and gas industry, heat exchangers, weldable pressure vessels and boilers
For more information in 13CrMoV9-10 steel grade in the following:
13CrMoV9-10 Chemical composition cast analysis
Element | 13CrMoV9-10 Max % | Element | 13CrMoV9-10 max % |
C | 0.11-0.15 | Cr | 2.0-2.50 |
Si | 0.10 | Cu | 0.20 |
Mn | 0.30-0.60 | Mo | 0.90-1.10 |
P | 0.015 | Nb | 0.07 |
S | 0.005 | Ni | 0.25 |
| | Ti | 0.03 |
N | 0.01 | V | 0.25-0.35 |
13CrMoV9-10 Mechanical properties
Grade | Condition | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | ||
| | | | -20 degree | ||
13CrMoV9-10 | +NT OR +QT | ≤ 16 | 455 | 600-780 | 18 | 27 |
16> to ≤40 | 488 | 600-780 | 18 | 27 | ||
40> to ≤60 | 488 | 600-780 | 18 | 27 | ||
60> to ≤100 | 435 | 590-770 | 18 | 27 | ||
100> to ≤150 | 435 | 590-770 | 18 | 27 | ||
150> to ≤250 | 415 | 580-760 | 18 | 27 |
Noted: +NT mean Normalized and tempered; +QT mean Quenched and tempered