New Products /back


20MnMoNi4-5,20MnMoNi4-5 steel,EN10028-2

2011年4月14日 by admin

EN10028-2,20MnMoNi4-5,Grade 20MnMoNi4-5,20MnMoNi4-5 steel,20MnMoNi4-5 steel plate

 

Adopt Standard: EN10028-2

Grade:P235GH,P265GH,P295GH,P355GH,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4,20MnMoNi4-5,15NiCuMoNb5-6-4,13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.

 

20MnMoNi4-5 steel grade

20MnMoNi4-5 steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.

In accordance with en10020, 20MnMoNi4-5 steel grade is alloy special steels.

20MnMoNi4-5 Grade delivery condition is normalized and tempered or quenched and tempered.

 

Gangsteel could supply 20MnMoNi4-5 steel grade in super thick steel plate for fabricators serving the oil and gas industry, heat exchangers, weldable pressure vessels and boilers

For more information in 20MnMoNi4-5 steel grade in the following:


20MnMoNi4-5 Chemical composition cast analysis

Element

20MnMoNi4-5  Max %

Element

20MnMoNi4-5 max %

C

0.15-0.23

Cr

0.20

Si

0.40

Cu

0.20

Mn

0.10-1.50

Mo

0.45-0.60

P

0.020

Nb

 

S

0.010

Ni

0.40-0.80

AL

 

Ti

 

N

0.012

V

0.02

 

20MnMoNi4-5 Mechanical properties

Grade

Condition

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

20MnMoNi4-5

+QT

≤ 16

470

590-750

18

27

16> to ≤40

  470

590-790

18

27

40> to ≤60

470

590-730

18

27

60> to ≤100

450

570-710

18

27

100> to ≤150

440

570-710

18

27

150> to ≤250

400

560-700

18

27

Noted: +NT mean Normalized and tempered; +QT mean Quenched and tempered

 

If you want to find our stock in 20MnMoNi4-5 or inquiry from our gangsteel, please feel free to contact us by email or calling.


 

Tags: EN10028-2  20MnMoNi4-5  Grade 20MnMoNi4-5  20MnMoNi4-5 steel  20MnMoNi4-5 steel plate  