EN10028-2 16Mo3 boiler and pressure vessel steel plate
2013年9月11日 by admin
EN10028-2 16Mo3 boiler and pressure vessel steel plate
Related Grade:P235GH,P265GH,P295GH,P355GH,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4,20MnMoNi4-5,15NiCuMoNb5-6-4,
13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.
16Mo3 steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.
In accordance with en10020, 16Mo3 steel grade is alloy special steels.
16Mo3 Grade delivery condition is Normalized or normalized and tempered or quenched and tempered.
Gangsteel could supply 16Mo3 steel grade in super thick steel plate for fabricators serving the oil and gas industry,
heat exchangers, weldable pressure vessels and boilers
Steel Services: Cutting, Painting, Pretreatment, Ultrasonic Test, Third Party Inspection, HIC, NACE, and so on.
16Mo3 Chemical composition cast analysis
Element | 16Mo3 Max % | Element | 16Mo3 max % |
C | 0.12-0.20 | Cr | 0.30 |
Si | 0.35 | Cu | 0.30 |
Mn | 0.40-0.90 | Mo | 0.25-0.35 |
P | 0.025 | Nb | |
S | 0.010 | Ni | |
AL | | Ti | 0.30 |
N | 0.012 | V | 0.02 |
16Mo3 Mechanical properties
Grade | Condition | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | ||
| | | | +20 degree | ||
16Mo3 | Normalized | ≤ 16 | 275 | 440-590 | 22 | 31 |
16> to ≤40 | 270 | 440-590 | 22 | 31 | ||
40> to ≤60 | 260 | 440-590 | 22 | 31 | ||
60> to ≤100 | 240 | 430-560 | 22 | 31 | ||
100> to ≤150 | 220 | 420-570 | 22 | 31 | ||
150> to ≤250 | 210 | 410-570 | 22 | 31 |
If you want to find our stock in 16Mo3 or inquiry from our gangsteel, please feel free to contact us by email or calling.
Yours sincerely,
Ms. Olina
Henan Gang Iron and Steel Co., Ltd
Tel: 86-0371-88884766
Fax: 86-0371-88884766
Cell: 86-15226033579
Email: olina@gangsteel.com
Skype: gangsteel18
0 Comments, 0 Trackbacks