EN10028-2 P265GH boiler and pressure vessel steel plate
2013年9月11日 by admin
EN10028-2 P265GH steel plate
Related Grade:P235gh,p265gh,p295gh,p355gh,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4, 20MnMoNi4-5,15NiCuMoNb5-6-4,
13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.
P235GH steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.
In accordance with en10020, P235gh,p265gh, p295gh and p355gh are non alloy quality steels.
All of other grade are alloy special steels.
P235GH Grade delivery condition is normalizing or be replaced with normalizing rolling at the discretion of manufactures.
Gangsteel could supply P235GH steel grade in super thick steel plate for fabricators serving the oil and gas industry,
heat exchangers, weldable pressure vessels and boilers
Steel Services: Cutting, Painting, Pretreatment, Ultrasonic Test, Third Party Inspection, HIC, NACE, and so on.
P235GH Chemical composition cast analysis
Element | P235GH Max % | Element | P235GH max % |
C | 0.16 | Cr | 0.30 |
Si | 0.35 | Cu | 0.30 |
Mn | 0.60-1.20 | Mo | 0.08 |
P | 0.015 | Nb | 0.020 |
S | 0.015 | Ni | 0.30 |
AL | 0.020 min | Ti | 0.30 |
N | 0.012 | V | 0.02 |
P235GH Mechanical properties
Type | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | -20 degree | |
Normalized | ≤ 16 | 235 | 360-480 | 24 | 27 |
16> to ≤40 | 225 | 360-480 | 24 | 27 | |
40> to ≤60 | 215 | 360-480 | 24 | 27 | |
60> to ≤100 | 200 | 360-480 | 24 | 27 | |
100> to ≤150 | 185 | 350-480 | 24 | 27 | |
150> to ≤250 | 170 | 340-480 | 24 | 27 |