New Products /back


X10CrMoVNb9-1,X10CrMoVNb9-1 steel plate

2011年4月14日 by admin

X10CrMoVNb9-1,X10CrMoVNb9-1,X10CrMoVNb9-1,X10CrMoVNb9-1

 

Adopt Standard: EN10028-2

Grade:P235GH,P265GH,P295GH,P355GH,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4,20MnMoNi4-5,15NiCuMoNb5-6-4,13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.

 

X10CrMoVNb9-1 steel grade

X10CrMoVNb9-1 steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.

In accordance with en10020, X10CrMoVNb9-1 steel grade is alloy special steels.

X10CrMoVNb9-1 Grade delivery condition is normalized and tempered or quenched and tempered.

 

Gangsteel could supply X10CrMoVNb9-1 steel grade in super thick steel plate for fabricators serving the oil and gas industry, heat exchangers, weldable pressure vessels and boilers

For more information in X10CrMoVNb9-1 steel grade in the following:


X10CrMoVNb9-1 Chemical composition cast analysis

Element

X10CrMoVNb9-1  Max %

Element

X10CrMoVNb9-1 max %

C

0..08-0.12

Cr

8.00-9.50

Si

0.50

Cu

0.30

Mn

0.30-0.60

Mo

0.85-1.05

P

0.020

Nb

0.06-0.10

S

0.005

Ni

0.30

AL

0.040

Ti

 

N

0.030-0.070

V

0.18-0.25

 

X10CrMoVNb9-1 Mechanical properties

Grade

Condition

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

X10CrMoVNb9-1

+QT OR NT

≤ 16

445

580-760

18

27

16> to ≤40

  445

580-760

18

27

40> to ≤60

445

580-760

18

27

60> to ≤100

435

550-730

18

27

100> to ≤150

435

550-730

18

27

150> to ≤250

435

520-700

18

27

Noted: +NT mean Normalized and tempered; +QT mean Quenched and tempered

 