New Products /back


X12CrMo5,X12CrMo5 steel plate,EN10028-2

2011年4月14日 by admin

EN10028-2,X12CrMo5,X12CrMo5,X12CrMo5,X12CrMo5

 

Adopt Standard: EN10028-2

Grade:P235GH,P265GH,P295GH,P355GH,16Mo3,18MnMo4-5,20MnMoNi4-5,15NiCuMoNb5-6-4,20MnMoNi4-5,15NiCuMoNb5-6-4,13CrMo4-5,13CrMoSi5-5,10CrMo9-10,12CrMo9-10,X12CrMo5,13CrMoV9-10,12CrMoV12-10,X10CrMoVNb9-1.

 

X12CrMo5 steel grade

X12CrMo5 steel grade is one of grade in En10028-2, which is non alloy and alloy steels with specified elevated temperature properties.

In accordance with en10020, X12CrMo5 steel grade is alloy special steels.

X12CrMo5 Grade delivery condition is normalized and tempered or quenched and tempered.

 

Gangsteel could supply X12CrMo5 steel grade in super thick steel plate for fabricators serving the oil and gas industry, heat exchangers, weldable pressure vessels and boilers

For more information in X12CrMo5 steel grade in the following:


X12CrMo5 Chemical composition cast analysis

Element

X12CrMo5  Max %

Element

X12CrMo5 max %

C

0.10-0.15

Cr

4.0-6.0

Si

0.50

Cu

0.30

Mn

0.30-0.60

Mo

0.45-0.65

P

0.020

Nb

 

S

0.005

Ni

0.30

AL

 

Ti

 

N

0.012

V

 

 

X12CrMo5 Mechanical properties

Grade

Condition

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-0 degree

X12CrMo5

+NT OR +QT

≤ 16

320

510-690

20

27

16> to ≤40

  320

510-690

20

27

40> to ≤60

320

510-690

20

27

60> to ≤100

300

480-660

20

27

100> to ≤150

 300

480-660

20

27

150> to ≤250

 300

450-630

20

27

Noted: +NT mean Normalized and tempered; +QT mean Quenched and tempered

 