New Products /back


P275NL1, P275NL1 steel plate,P275NL1 Grade,EN10028-3 P275NL1

2011年4月14日 by admin

 

Adopt Standard EN10028-3

Related grades we could supply:

EN10028-3 boiler and pressure vessel steel plate

P275NH

P275NL1

P275NL2

P355N

P355NH

P355NL1

P355NL2

P460NH

P460NL1

P460NL2

 

P275NL1 steel grade is a normalized, weldable fine grain steels for pressure purposed. The dimensions and tolerance on dimensions should be according to EN 10028-1.

 

P…N mean the room temperature, P…NH means the elevated temperature quality
P…NL1 means the low temperature quality, P…NL2 means the special low temperature quality.

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we could supply the min order is one steel plate and promise the competitive price in order to enlarge our oversea market.


P275NL1 Chemical composition cast analysis:

Element

P275NL1  Max %

Element

P275NL1 max %

C

0.16

Cr

0.30

Si

0.40

Cu

0.30

Mn

0.80-1.50

Mo

0.08

P

0.020

Nb

0.050

S

0.010

Ni

0.50

AL

0.020

Ti

0.03

N

0.012

V

0.05

 

P275NL1 Mechanical properties:

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-40 degree

P275NL1

Normalized

≤ 16

275

390-510

24

27

16> to ≤40

265

390-510

24

27

40> to ≤60

255

390-510

24

27

60> to ≤100

235

370-490

23

27

100> to ≤150

225

360-480

23

27

150> to ≤250

215

350-470

23

27

 

To find more about P275NL1 or inquiry from our gangsteel, please feel free to contact us by email or calling.

 