New Products /back


P355NL1, P355NL1 steel plate,EN10028-3 P355NL1

2011年4月14日 by admin

 

Adopt Standard EN10028-3

Related grades we could supply:

EN10028-3 boiler and pressure vessel steel plate

P275NH

P275NL1

P275NL2

P355N

P355NH

P355NL1

P355NL2

P460NH

P460NL1

P460NL2

 

P355NL1 steel grade is a normalized, weldable fine grain steels for pressure purposed. The dimensions and tolerance on dimensions should be according to EN 10028-1.

 

P…N mean the room temperature, P…NH means the elevated temperature quality
P…NL1 means the low temperature quality, P…NL2 means the special low temperature quality.

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we could supply the min order is one steel plate and promise the competitive price in order to enlarge our oversea market.


P355NL1 Chemical composition cast analysis:

Element

P355NL1  Max %

Element

P355NL1 max %

C

0.18

Cr

0.30

Si

0.50

Cu

0.30

Mn

1.10-1.70

Mo

0.08

P

0.025

Nb

0.050

S

0.015

Ni

0.50

AL

0.020

Ti

0.03

N

0.012

V

0.01

 

P355NL1 Mechanical properties:

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-40 degree

P355NL1

Normalized

≤ 16

355

490-630

22

27

16> to ≤40

345

490-630

22

27

40> to ≤60

335

490-630

22

27

60> to ≤100

315

470-610

21

27

100> to ≤150

305

460-600

21

27

150> to ≤250

295

450-590

21

27

 

To find more about P355NL1 or inquiry from our gangsteel, please feel free to contact us by email or calling.

 

Tags: P355NL1  P355NL1 steel plate  P355NL1 Grade  EN10028-3 P355NL1.  