P460NL1, P460NL1 steel plate,EN10028-3 P460NL1
2011年4月14日 by admin
Adopt Standard EN10028-3
Related grades we could supply:
EN10028-3 boiler and pressure vessel steel plate | ||||
P460NL1 steel grade is a normalized, weldable fine grain steels for pressure purposed. The dimensions and tolerance on dimensions should be according to EN 10028-1.
P…N mean the room temperature, P…NH means the elevated temperature quality
P…NL1 means the low temperature quality, P…NL2 means the special low temperature quality.
Gangsteel is a large agent of HBIS wuyang mill in
P460NL1 Chemical composition cast analysis:
Element | P460NL1 Max % | Element | P460NL1 max % |
C | 0.20 | Cr | 0.30 |
Si | 0.60 | Cu | 0.70 |
Mn | 1.10-1.70 | Mo | 0.10 |
P | 0.025 | Nb | 0.05 |
S | 0.015 | Ni | 0.80 |
| 0.020 | Ti | 0.03 |
N | 0.025 | V | 0.20 |
P460NL1 Mechanical properties:
Grade | Type | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | ||
| | | | -40 degree | ||
P460NL1 | Normalized | ≤ 16 | 460 | 570-720 | 17 | 27 |
16> to ≤40 | 445 | 570-720 | 17 | 27 | ||
40> to ≤60 | 430 | 570-720 | 17 | 27 | ||
60> to ≤100 | 400 | 540-710 | 17 | 27 | ||
100> to ≤150 | 400 | 540-710 | 17 | 27 | ||
150> to ≤250 | 400 | 540-710 | 17 | 27 |
To find more about P460NL1 or inquiry from our gangsteel, please feel free to contact us by email or calling.
Tags: P460NL1 P460NL1 steel plate P460NL1 Grade EN10028-3 P460NL1.