Adopt Standard EN10028-5

Related grades we could supply:

EN10028-5 boiler and pressure vessel steel plate

P355M

P355ML1

P355ML2

P420M

P420ML1

P420ML2

P460M

P460ML1

P460ML2

 

 

P355ML2 is a thermo mechanically rolled and weldable fine grain steels grade. The dimensions and tolerance on dimensions should be according to EN 10028-1. P355ML2 Grade usual be used for pressure equipments.

 

P…M mean the -20 degree and the impact energy is 27J

P…ML1 means the -40 temperature quality and the impact energy is 27J
P…NL2 means the -50 temperature quality and the impact energy is 27J

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we have enough technology to produce research and develop new grade for our customers. We are using our best service, faster delivery and more competitive price to enlarge our oversea market.

 

P355ML2 Chemical composition cast analysis:

Element

P355ML2  Max %

Element

P355ML2 max %

C

0.14

Mo

0.20

Si

0.50

Nb

00.05

Mn

1.60

Ni

0.50

P

0.020

TI

0.05

S

0.015

Vi

0.10

AL

0.020 min

 

 

N

0.015

 

 

 

P355ML2 Mechanical properties:

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-50 degree

P355ML2

Normalized

≤ 16

355

450-610

22

27

16> to ≤40

355

450-610

22

27

40> to ≤63

345

450-610

22

27

 

To find more about P355ML2 or inquiry from our gangsteel, please feel free to contact us by email or calling.

 

Tags: P355ML2  P355ML2 Grade  P355ML2 steel plate  P355ML2  EN10028-5  