Adopt Standard EN10028-5

Gang steel Grade:

EN10028-5

Grade

Grade

Grade

Grade

P355M

P355ML1

P355ML2

P420M

P420ML1

P420ML2

P460M

P460ML1

P460ML2

 

 

P420M steel plate

 

P420M is a thermo mechanically rolled and weldable fine grain steels grade. The dimensions and tolerance on dimensions should be according to EN 10028-1. P420M Grade usual be used for pressure equipments.

 

P…M mean the -20 degree and the impact energy is 27J

P…ML1 means the -40 temperature quality and the impact energy is 27J
P…NL2 means the -50 temperature quality and the impact energy is 27J

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we have enough technology to produce research and develop new grade for our customers. We are using our best service, faster delivery and more competitive price to enlarge our oversea market.

 

P420M Chemical composition cast analysis

Element

P420M  Max %

Element

P420M max %

C

0.16

Mo

0.20

Si

0.50

Nb

00.05

Mn

1.70

Ni

0.50

P

0.025

TI

0.05

S

0.020

Vi

0.10

AL

   0.020 min

 

 

N

0.020

 

 

 

 

P420M Mechanical properties,                     Longitudinal min impact energy

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

P420M

Normalized

≤ 16

420

500-660

19

27

16> to ≤40

400

500-660

19

27

40> to ≤63

390

500-660

19

27

 

If you want to find our stock in P420M or inquiry from our gangsteel, please feel free to contact us by email or calling.

 

P420M,P420M Grade,P420M steel plate,P420M,EN10028-5

 

 

Tags: P420M  P420M Grade  P420M steel plate  P420M  EN10028-5  

0 Comments, 0 Trackbacks