New Products /back


P420ML1,P420ML1 Grade,P420ML1 steel plate,P420ML1,EN10028-5

2011年4月14日 by admin

 

Adopt Standard EN10028-5

Related grades we could supply:

EN10028-5 boiler and pressure vessel steel plate

P355M

P355ML1

P355ML2

P420M

P420ML1

P420ML2

P460M

P460ML1

P460ML2

 

 

P420ML1 is a thermo mechanically rolled and weldable fine grain steels grade. The dimensions and tolerance on dimensions should be according to EN 10028-1. P420ML1 Grade usual be used for pressure equipments.

 

P…M mean the -20 degree and the impact energy is 27J

P…ML1 means the -40 temperature quality and the impact energy is 27J
P…NL2 means the -50 temperature quality and the impact energy is 27J

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we have enough technology to produce research and develop new grade for our customers. We are using our best service, faster delivery and more competitive price to enlarge our oversea market.

 

P420ML1 Chemical composition cast analysis:

Element

P420ML1  Max %

Element

P420ML1 max %

C

0.16

Mo

0.20

Si

0.50

Nb

00.05

Mn

1.70

Ni

0.50

P

0.020

TI

0.05

S

0.015

Vi

0.10

AL

0.020 min

 

 

N

0.020

 

 

 

 

P420ML1 Mechanical properties:

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-40 degree

P420ML1

Normalized

≤ 16

420

500-660

19

27

16> to ≤40

400

500-660

19

27

40> to ≤63

390

500-660

19

27

 

To find more about P420ML1 or inquiry from our gangsteel, please feel free to contact us by email or calling.

 

Tags: P420ML1  P420ML1 Grade  P420ML1 steel plate  P420ML1  EN10028-5  