New Products /back


P460M,P460M Grade,P460M steel plate,P460M,EN10028-5

2011年4月14日 by admin

 

Adopt Standard EN10028-5

Related grades we could supply:

EN10028-5 boiler and pressure vessel steel plate

P355M

P355ML1

P355ML2

P420M

P420ML1

P420ML2

P460M

P460ML1

P460ML2

 

 

P460M is a thermo mechanically rolled and weldable fine grain steels grade. The dimensions and tolerance on dimensions should be according to EN 10028-1. P460M Grade usual be used for pressure equipments.

 

P…M mean the -20 degree and the impact energy is 27J

P…ML1 means the -40 temperature quality and the impact energy is 27J
P…NL2 means the -50 temperature quality and the impact energy is 27J

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we have enough technology to produce research and develop new grade for our customers. We are using our best service, faster delivery and more competitive price to enlarge our oversea market.

 

P460M Chemical composition cast analysis:

Element

P460M  Max %

Element

P460M max %

C

0.16

Mo

0.20

Si

0.60

Nb

00.05

Mn

1.70

Ni

0.50

P

0.025

TI

0.05

S

0.020

Vi

0.10

AL

0.020 min

 

 

N

0.020

 

 

 

 

P460M Mechanical properties:

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

P460M

Normalized

≤ 16

460

530-720

17

27

16> to ≤40

440

530-720

17

27

40> to ≤63

430

530-720

17

27

 

To find more about P460M or inquiry from our gangsteel, please feel free to contact us by email or calling.

 

Tags: P460M  P460M Grade  P460M steel plate  P460M  EN10028-5  

0 Comments, 0 Trackbacks