P460ML1 is a thermo mechanically rolled and weldable fine grain steels grade. The dimensions and tolerance on dimensions should be according to EN 10028-1. P460ML1 Grade usual is used for pressure equipments.

 

P…M mean the -20 degree and the impact energy is 27J

P…ML1 means the -40 temperature quality and the impact energy is 27J
P…NL2 means the -50 temperature quality and the impact energy is 27J

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we have enough technology to produce research and develop new grade for our customers. We are using our best service, faster delivery and more competitive price to enlarge our oversea market.

 

P460ML1 Chemical composition cast analysis:

Element

P460ML1  Max %

Element

P460ML1 max %

C

0.16

Mo

0.20

Si

0.60

Nb

00.05

Mn

1.70

Ni

0.50

P

0.020

TI

0.05

S

0.015

Vi

0.10

AL

0.020 min

 

 

N

0.020

 

 

 

 

P460ML1 Mechanical properties:

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-40 degree

P460ML1

Normalized

≤ 16

460

530-720

17

27

16> to ≤40

440

530-720

17

27

40> to ≤63

430

530-720

17

27

 

To find more about P460ML1 or inquiry from our gangsteel, please feel free to contact us by email or calling.

 