New Products /back


EN10028-6 P500Q quenched and tempered steel plate

2013年9月6日 by admin

P500Q,P500Q steel plate,P500Q steel grade,EN10028-6 P500Q

 

Adopt Standard EN 10028-6

Gang steel Grade:

EN10028-6

P355Q

P355QH

P355QL1

P355QL2

P460Q

P460QH

P460QL1

P460QL2

P500Q

P500QH

P500QL1

P500QL2

P690Q

P690QL1

P690QL2

 

 

 

 


P500Q Steel plate

P500Q steel grade is quenched and tempered steel grade for weldable fine grain pressure purposes.
P500Q Grade has a good weldable and used in high temperature equipment and pressure vessel.

 

P…Q means the -20 degree and the impact energy is 27J

P…QH means the -20 temperature quality and the impact energy is 27J
P…QL1 means the -40 temperature quality and the impact energy is 27J

P…QL2 means the -60 temperature quality and the impact energy is 27J 

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we have enough technology to produce research and develop new grade for our customers. We are using our best service, faster delivery and more competitive price to enlarge our oversea market.

 

P500Q Chemical composition cast analysis

Element

P500Q  Max %

Element

P500Q max %

C

0.18

Cr

1.00

Si

0.60

Mo

0.70

Mn

1.70

Cu

0.30

P

0.025

Nb

0.05

S

0.015

Ni

         1.50

N

0.015 

TI

0.05

B

0.005

V

0.08



 

            

P500Q Mechanical properties,                     longitudinal min impact energy

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

P500Q

+QT

≤ 50

500

590-770

17

27

50to ≤100

480

590-770

17

27

100o ≤150

440

540-720

17

27



If you want to find our stock in P500Q or inquiry from our gangsteel, please feel free to contact us by email or calling.

Tags: P500Q  P500Q steel plate  P500Q steel grade  EN10028-6  P500Q  EN 10028-6 P500Q  P500Q steel supplier  P500Q price  