New Products /back


EN10028-6 P500QH quenched and tempered steel plate

2013年9月6日 by admin

 

 Adopt Standard EN 10028-6

Gang steel Grade:

EN10028-6

P355Q

P355QH

P355QL1

P355QL2

P460Q

P460QH

P460QL1

P460QL2

P500Q

P500QH

P500QL1

P500QL2

P690Q

P690QL1

P690QL2

 

 

 

 

 

P500QH steel grade is quenched and tempered steel grade for weldable fine grain pressure purposes.
P500QH Grade has a good weldable and used in high temperature equipment and pressure vessel.

 

P…Q means the -20 degree and the impact energy is 27J

P…QH means the -20 temperature quality and the impact energy is 27J
P…QL1 means the -40 temperature quality and the impact energy is 27J

P…QL2 means the -60 temperature quality and the impact energy is 27J

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we have enough technology to produce research and develop new grade for our customers. We are using our best service, faster delivery and more competitive price to enlarge our oversea market.

 

P500QH Chemical composition cast analysis

Element

P500QH  Max %

Element

P500QH max %

C

0.18

Cr

1.00

Si

0.60

Mo

0.70

Mn

1.70

Cu

0.30

P

0.025

Nb

0.05

S

0.015

Ni

         1.50

N

0.015

TI

0.05

B

0.005

V

0.08

           

P500QH Mechanical properties,                     longitudinal min impact energy

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

P500QH

+QT

≤ 50

500

590-770

17

27

50to ≤100

480

590-770

17

27

100o ≤150

440

540-720

17

27

 

If you want to find our stock in P500QH or inquiry from our gangsteel, please feel free to contact us by email or calling.

 

 