EN10028-6 P690QH quenched and tempered steel plate

2013年9月9日 by admin

P690QH,P690QH steel plate,P690QH steel grade,EN10028-6 P690QH

 

Adopt Standard EN 10028-6

Gang steel Grade:

P355Q,P355QH,P355QL1,P355QL2,P460Q,P460QH,P460QL1,P460QL2,P500Q,P500QH,P500QL1,P500QL2,P690Q,P690QH,P690QL1,P690QL2


P690QH Steel plate

 

P690QH steel grade is quenched and tempered steel grade for weldable fine grain pressure purposes.
P690QH Grade has a good weldable and used in high temperature equipment and pressure vessel.

 

P…Q means the -20 degree and the impact energy is 27J

P…QH means the -20 temperature quality and the impact energy is 27J
P…QL1 means the -40 temperature quality and the impact energy is 27J

P…QL2 means the -60 temperature quality and the impact energy is 27J 

 

Gangsteel is a large agent of HBIS wuyang mill in China and we are specialized in super thick steel plate. So, we have enough technology to produce research and develop new grade for our customers. We are using our best service, faster delivery and more competitive price to enlarge our oversea market.

 

P690QH Chemical composition cast analysis

Element

P690QH  Max %

Element

P690QH max %

C

0.20

Cr

1.50

Si

0.80

Mo

0.70

Mn

1.70

Cu

0.30

P

0.025

Nb

0.06

S

0.015

Ni

         2.50

N

0.015 

TI

0.05

B

0.005

V

0.12


            

P690QH Mechanical properties,                     longitudinal min impact energy

Grade

Type

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

P690QH

+QT

≤ 50

690

770-940

14

27

50to ≤100

670

770-940

14

27

100o ≤150

630

720-900

14

27