New Products /back


28Mn6|EN 10083-2 28Mn6 Quenching and Tempering Steel Plate

2013年7月23日 by admin

28Mn6|EN 10083-2 28Mn6 Quenching and Tempering Steel Plate

 

The 28Mn6 has reliable mechanical property, good formability and excellent cutability performance, which is widely used in various industries, such as architecture, bridge construction, marine craft, heavy machine and other structure parts.

 

28Mn6 is a structural grade steel, offering good tensile and yield strength, also used in bolt, nut and lever ect.

 

Available size:

Thickness: 2.4mm--5mm

Width:  900mm--1750mm

Length: 2000mm to 12000mm

 

Gangsteel is specialized in supplying steel plate in 28Mn6 from stock or directly from the mill to customer destinations on global footing.

 

For more information of 28Mn6 steel plates, please refer to the technical information below:

 

28Mn6 Chemical composition

Grade

The Element Max (%)

28Mn6

C

Si

Mn

P

S

0.25-0.32

0.40

1.30-1.65

0.030

0.035

Cr

Mo

Ni

Cr+Mo+Ni

 

0.40

0.10

0.40

0.63

 

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Mechanical property:

Grade

thickness

Yield

Tensile

Elongation

28Mn6

 

mm

Min Mpa

Mpa

Min  %

t≤8

≥590

800-950

≥13

8--20

≥490

700-850

≥15

20-60

≥440

650-800

≥16

Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate

 

If you have any need 28Mn6 steel plate, please feel free to contact us soon. We sincerely hope old and 

new customers to visit our mill for a long steel business.

Tags: 28Mn6  EN 10083-2 28Mn6  28Mn6 steel  28Mn6 steel plate  

0 Comments, 0 Trackbacks