C22E|EN 10083-2 C22E Quenching and Tempering Steel Plate
2013年7月23日 by admin
C22E|EN 10083-2 C22E Quenching and Tempering Steel Plate
The C22E has reliable mechanical property, good formability and excellent cutability performance, which is widely used in various industries, such as architecture, bridge construction, marine craft, heavy machine and other structure parts.
C22E is a structural grade steel, offering good tensile and yield strength, also used in bolt, nut and lever ect.
Gangsteel is specialized in supplying steel plate in C22E from stock or directly from the mill to customer destinations on global footing.
For more information of C22E steel plates, please refer to the technical information below:
C22E Chemical composition | |||||
Grade | The Element Max (%) | ||||
C22E | C | Si | Mn | P | S |
0.17-0.24 | 0.40 | 0.40-0.70 | 0.030 | 0.035 | |
Cr | Mo | Ni | Cr+Mo+Ni | | |
0.40 | 0.10 | 0.40 | 0.63 | |
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
Mechanical property:
Grade | thickness | Yield | Tensile | Elongation |
C22E | mm | Min Mpa | Mpa | Min % |
t≤8 | ≥340 | 850-1000 | ≥20 | |
8--20 | ≥290 | 470-620 | ≥22 | |
20-60 | | | |
Shipbuilding steel plate| Alloy steel plates| High strength plate| Carbon steel plate| Stainless steel plate
If you have any need C22E steel plate, please feel free to contact us soon. We sincerely hope old and
new customers to visit our mill for a long steel business.
Tags: C22E EN 10083-2 C22E C22E steel C22E steel plate
0 Comments, 0 Trackbacks