New Products /back


C35E|EN 10083-2 C35E Quenching and Tempering Steel Plate

2013年7月23日 by admin

C35E|EN 10083-2 C35E Quenching and Tempering Steel Plate

 

The C35E has reliable mechanical property, good formability and excellent cutability performance, which is widely used in various industries, such as architecture, bridge construction, marine craft, heavy machine and other structure parts.

 

C35E is a structural grade steel, offering good tensile and yield strength, also used in bolt, nut and lever ect.

 

Gangsteel is specialized in supplying steel plate in C35E from stock or directly from the mill to customer destinations on global footing.

 

For more information of C35E steel plates, please refer to the technical information below:

 

C35E Chemical composition

Grade

The Element Max (%)

C35E

C

Si

Mn

P

S

0.32-0.39

0.40

0.50-0.80

0.030

0.035

Cr

Mo

Ni

Cr+Mo+Ni

 

0.40

0.10

0.40

0.63

 

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Mechanical property:

Grade

thickness

Yield

Tensile

Elongation

 C35E

mm

Min Mpa

Mpa

Min  %

t≤8

≥430

630-780

≥17

8--20

≥380

 600-750

≥19

20-60

≥320

550-700

≥20

Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate

 

If you have any need C35E steel plate, please feel free to contact us soon. We sincerely hope old and 

new customers to visit our mill for a long steel business

Tags: C35E  EN 10083-2 C35E  C35E steel plate  EN 10083-2 steel  

0 Comments, 0 Trackbacks