C35|EN 10083-2 C35 Quenching and Tempering Steel Plate

 

The C35 has reliable mechanical property, good formability and excellent cutability performance, which is widely used in various industries, such as architecture, bridge construction, marine craft, heavy machine and other structure parts.

 

C35 is a structural grade steel, offering good tensile and yield strength, also used in bolt, nut and lever ect.

 

Gangsteel is specialized in supplying steel plate in C35 from stock or directly from the mill to customer destinations on global footing.

 

For more information of C35 steel plates, please refer to the technical information below:

 

C35 Chemical composition

Grade

                The Element Max (%)

 

C35

C

Si

Mn

P

S

0.32-0.39

0.40

0.50-0.80

0.045

0.045

Cr

Mo

Ni

Cr+Mo+Ni

 

0.40

0.10

0.40

0.63

 

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Mechanical property:

Grade

Heatment

Yield

Tensile

Elongation

 C35

 

 

Min Mpa

Mpa

Min  %

N

≥300

≥550

≥18

QT

≥430

  630--780

≥17

Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate

 

If you have any need C35 steel plate, please feel free to contact us soon. We sincerely hope old and 

new customers to visit our mill for a long steel business.

Tags: C35  EN 10083-2 C35  C35 steel  C35 steel plate  EN 10083-2 steel  

0 Comments, 0 Trackbacks