New Products /back


C40E|EN 10083-2 C40E Quenching and Tempering Steel Plate

2013年7月23日 by admin

C40E|EN 10083-2 C40E Quenching and Tempering Steel Plate

 

The C40E has reliable mechanical property, good formability and excellent cutability performance, which is widely used in various industries, such as architecture, bridge construction, marine craft, heavy machine and other structure parts.

 

C40E is a structural grade steel, offering good tensile and yield strength, also used in bolt, nut and lever ect.

 

Gangsteel is specialized in supplying steel plate in C40E from stock or directly from the mill to customer destinations on global footing.

 

For more information of C40E steel plates, please refer to the technical information below:

 

C40E Chemical composition

Grade

The Element Max (%)

C40E

C

Si

Mn

P

S

0.37-0.44

0.40

0.50-0.80

0.030

0.035

Cr

Mo

Ni

Cr+Mo+Ni

 

0.40

0.10

0.40

0.63

 

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Mechanical property:

Grade

thickness

Yield

Tensile

Elongation

 C40E

 

mm

Min Mpa

Mpa

Min  %

t≤8

≥460

650-800

≥16

8--20

≥400

  630-780

≥18

20-60

≥350

600-750

≥19

Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate

 

If you have any need C40E steel plate, please feel free to contact us soon. We sincerely hope old and 

new customers to visit our mill for a long steel business.

Tags: C40E  EN 10083-2 C40E  C40E steel grade  EN 10083-2 steel  

0 Comments, 0 Trackbacks