C45|EN 10083-2 C45 Quenching and Tempering Steel Plate

2013年7月23日 by admin

C45|EN 10083-2 C45 Quenching and Tempering Steel Plate

 

The C45 has reliable mechanical property, good formability and excellent cutability performance, which is widely used in various industries, such as architecture, bridge construction, marine craft, heavy machine and other structure parts.

 

C45 is a structural grade steel, offering good tensile and yield strength, also used in bolt, nut and lever ect.

 

Gangsteel is specialized in supplying steel plate in C45 from stock or directly from the mill to customer destinations on global footing.

 

For more information of C45 steel plates, please refer to the technical information below:

 

C45 Chemical composition

Grade

The Element Max (%)

C45

C

Si

Mn

P

S

0.42-0.50

0.40

0.50-0.80

0.045

0.045

Cr

Mo

Ni

Cr+Mo+Ni

 

0.40

0.10

0.40

0.63

 

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Mechanical property:

Grade

thickness

Yield

Tensile

Elongation

 C45

 

mm

Min Mpa

Mpa

Min  %

t≤8

≥490

700-850

≥14

8--20

≥430

  650-800

≥16

20-60

≥370

630-780

≥17

Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate

 

If you have any need C45 steel plate, please feel free to contact us soon. We sincerely hope old and 

new customers to visit our mill for a long steel business.

Tags: C45  EN 10083-2 C45  C45 steel plate  EN 10083-2 steel  

0 Comments, 0 Trackbacks