New Products /back


C55R|EN 10083-2 C55R Quenching and Tempering Steel Plate

2013年7月23日 by admin

C55R|EN 10083-2 C55R Quenching and Tempering Steel Plate

 

The C55R has reliable mechanical property, good formability and excellent cutability performance, which is widely used in various industries, such as architecture, bridge construction, marine craft, heavy machine and other structure parts.

 

C55R is a structural grade steel, offering good tensile and yield strength, also used in bolt, nut and lever ect.

 

Gangsteel is specialized in supplying steel plate in C55R from stock or directly from the mill to customer destinations on global footing.

 

For more information of C55R steel plates, please refer to the technical information below:

 

C55R Chemical composition

Grade

The Element Max (%)

C55R

C

Si

Mn

P

S

0.52-0.60

0.40

0.60-0.90

0.030

0.020-0.040

Cr

Mo

Ni

Cr+Mo+Ni

 

0.40

0.10

0.40

0.63

 

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Mechanical property:

Grade

thickness

Yield

Tensile

Elongation

 C55R

 

mm

Min Mpa

Mpa

Min  %

t≤8

≥550

800-950

≥12

8--20

≥490

   750-900

≥14

20-60

≥420

700-850

≥15

Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate

 

If you have any need C55R steel plate, please feel free to contact us soon. We sincerely hope old and 

new customers to visit our mill for a long steel business.

Tags: C55R  EN 10083-2 C55R  C55R steel plate  C55R steel  

0 Comments, 0 Trackbacks