New Products /back


C60E|EN 10083-2 C60E Quenching and Tempering Steel Plate

2013年7月23日 by admin

C60E|EN 10083-2 C60E Quenching and Tempering Steel Plate

 

The C60E has reliable mechanical property, good formability and excellent cutability performance, which is widely used in various industries, such as architecture, bridge construction, marine craft, heavy machine and other structure parts.

 

C60E is a structural grade steel, offering good tensile and yield strength, also used in bolt, nut and lever ect.

 

Gangsteel is specialized in supplying steel plate in C60E from stock or directly from the mill to customer destinations on global footing.

 

For more information of C60E steel plates, please refer to the technical information below:

 

C60EE Chemical composition

Grade

The Element Max (%)

C60E

C

Si

Mn

P

S

0.57-0.65

0.40

0.60-0.90

0.030

0.035

Cr

Mo

Ni

Cr+Mo+Ni

 

0.40

0.10

0.40

0.63

 

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Mechanical property:

Grade

thickness

Yield

Tensile

Elongation

 C60E

 

mm

Min Mpa

Mpa

Min  %

t≤8

≥580

580-1000

≥11

8--20

≥520

  800-950

≥13

20-60

≥450

750-900

≥14

Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate

 

If you have any need C60E steel plate, please feel free to contact us soon. We sincerely hope old and 

new customers to visit our mill for a long steel business.

Tags: C60E  EN 10083-2 C60E  C60E steel plate  EN 10083-2 steel  

0 Comments, 0 Trackbacks